Main Discussion Area > ABO
ABO techniques, processes and tools.
soy:
I'll try to get the video of you with the antler billit in sd...
bowmo:
Track: Once you get the hang of abo and the proper edge prep your points shouldn't end up any thicker. I can take the same pressure flakes with antler as copper, you just have to press a little harder and dress your tools constantly.
iowabow:
Well I happen to have a point to show you from the stand this morning. Everyone who does ABO has different techniques in my case I never ever dress my pressure flaking tools now that I use a large and small ulna for notching. The ishi never ever gets touch until I make another one. I just made 40 points never dressed a tool. Zero maintenance other than replacement.
iowabow:
The point shown was built from coring not from a flake.
iowabow:
Forgot to add my process is not better just different from bowmo. I have seen his work good stuff. The only difference is I have a better PA name. >:D
Navigation
[0] Message Index
[#] Next page
[*] Previous page
Go to full version