bubby:
I got a little time between rain and got a couple file knives bevels ground. I heat them to past magnetic and just let them cool in the forge to anneal them first. I use salt to check as it melts at 1475 or right about there which is where you want it

burchett.donald:
       Looking good Bubby, like the blade design... (-P
                                                                                             Don

KHalverson:
Nice grinds.

bubby:
Thanks guys

Danzn Bar:
I like both styles, looks good.
DBar